Hi,

I'm currently making some translucent statuettes with the glasscast 50 but I'm a little bit in a rush.

Is it possible to accelerate the curing by putting the mold in an oven after the initial heat of the reaction has dissipated ?

How would be the curing times ? 

Thank you in advance
Reply
Desobrem
D
Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)
Group: Forum Members
Posts: 4, Visits: 42
Thank you for your answer Smile I will try that tomorrow. I hope it will work !