By Desobrem - 1/4/2019 3:48:05 PM
Hi,
I'm currently making some translucent statuettes with the glasscast 50 but I'm a little bit in a rush.
Is it possible to accelerate the curing by putting the mold in an oven after the initial heat of the reaction has dissipated ?
How would be the curing times ?
Thank you in advance
|
By Desobrem - 1/6/2019 6:42:21 PM
Thank you for your answer I will try that tomorrow. I hope it will work !
|
|