How much roughly and where in the UK could I have a mould taken of my bumper, now I normally make all my moulds but no sure I feel confident making one from this.
Thoughts on how hard it would be?
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Mould
111mattin111
-
7 Years Ago
Plenty of places here in the uk that could help. Biggest thing will be your budget and how many parts you want to make and in with what process? From a squint on my phone i reckon there wouldnt be to...
scottracing
-
7 Years Ago
I'm Nottinghamshire, do you think it would be easy enough to attempt myself, I normally resin infuse my parts.
111mattin111
-
7 Years Ago
If you've made any split moulds before then you can make this, it's not as difficult as the aggressive styling makes it appear. All those vents will have decent draft angles, so you just need to...
Hanaldo
-
7 Years Ago
I think like you say with it having aggressive lines and lots going on it's made me unsure if I'm up to it as I've never tried a part like this I've made split moulds in the past.
111mattin111
-
7 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search