	Group: Forum Members 	        
    Posts: 2.5K, 
    Visits: 28K 
    
 
          
		     | 
				                       
                 
                
                    
			            If you've made any split moulds before then you can make this, it's not as difficult as the aggressive styling makes it appear. 
  All those vents will have decent draft angles, so you just need to blank them off from behind. Might need a separate piece for the bottom of the front lip, and if you are keeping the returns on the inside if the wheel arches then they will need separate pieces as well. But the majority of this will be in one piece.                
			            				
			                                 
                     
                                            
                         
                    
                  
             |