Hi there, merry xmas everyone!
Lately my last 2 infusions have gone wrong,i have noticed that when my part is 95% finished i shut the resin line off and leave the vac line going to get rid of the excess trapped air.the whole infusion looks nice and clear but once the vac is on to long i notice the top section of my mold (near the resin inlet) it starts to go cloudy and i can see small bubbles forming everywhere coming up through my fibreglass,this section is thicker in reinforcement.
Am i leaving vacuum too long? it almost seems like the resin is boiling. I have degassed resin prior to infusion and i have 100% no leaks .
any help would be much appreciated,cheers