Group: Forum Members
Posts: 107,
Visits: 504
|
hi james,
i've used the 2 part rattle can primer and paint. we get it through bmw parts, we use it to colour the inside of panels before we bond and rivet them on. i would imagine it should be fine on foam as it contains very little thinners
|