By jamesw - 10/20/2012 5:24:15 PM

Been looking at this:

http://www.spraymax.de/index.php?id=351&L=1

Available in uk for £18 here: http://www.ukpaints.co.uk/spraymax.php?subsearch=spraymax

has an in can button that mixes the 2 part system, and contains no isocynates meaning with the right mask this is home safe...

Any used a 2 pack epoxy filler on foam - is it foam safe? any problems with solvents ruining mould release?

James
By neilb - 10/21/2012 5:38:57 AM

hi james,

i've used the 2 part rattle can primer and paint. we get it through bmw parts, we use it to colour the inside of panels before we bond and rivet them on. i would imagine it should be fine on foam as it contains very little thinners