Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
You can try using filleting wax or plasticine around the joins or worst case, flash tape but flash tape on the inside will leave slight lines where the edge of the tape is.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|