Steve Broad - 12/9/2018 3:48:29 PM
I am about to remake my roof, so have similar issues. At the moment my plan is to make a 3 piece mould, with the joins very close to the door recesses. Doing it this way keeps the main roof panel as a single piece, removing the risk of a join showing in the final part.

This is how I was thinking of maybe doing this mould the roof on one bit then both sides separate 

Steve Broad
Steve Broad
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
I am about to remake my roof, so have similar issues. At the moment my plan is to make a 3 piece mould, with the joins very close to the door recesses. Doing it this way keeps the main roof panel as a single piece, removing the risk of a join showing in the final part.
Furrari
F
Supreme Being (494 reputation)Supreme Being (494 reputation)Supreme Being (494 reputation)Supreme Being (494 reputation)Supreme Being (494 reputation)Supreme Being (494 reputation)Supreme Being (494 reputation)Supreme Being (494 reputation)Supreme Being (494 reputation)
Group: Awaiting Activation
Posts: 63, Visits: 99
Mechanical lock. Yes we’ve all had those.

In the 70's I was Project Engineer in charge the design of the inspection media for the T68 ( no it was an Australian Land Train not a Russian tank). Only had problems with one fixture. I worked out we could spring the panel out of the fixture so we wouldn’t need to go to the cost of a two part fixture. Well you could spring the panel, but you can’t spring a wooden buck. Whoops.
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
111mattin111 - 12/5/2018 7:43:06 AM
Will it have to be split mould? 
It's been done in the past 

The necessity for a split-mould seems pretty obvious - if you stood at the front of the car looking down the middle of the roof, the rebates for the door and the weather channel seem to undercut quite distinctly (just picture trying to lift that mould off the roof and door rebates!) which means you would need to either split the whole mould down the middle of the roof-line or have bolt-on/removable barriers at the edges that form the rebate and weather channel. 

Looking at the detail of the pressed steel around the door closure area and the weather tracks I would have thought that you might even need to do some smoothing out and simplifying of that detail too.


Matt Statham
Easy Composites / Carbon Mods - Technical Sales
111mattin111
111mattin111
Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)
Group: Forum Members
Posts: 67, Visits: 910
Will it have to be split mould? 
It's been done in the past 
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Definitely.
111mattin111
111mattin111
Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)
Group: Forum Members
Posts: 67, Visits: 910
Hi guys just about to take a mould of my roof the only bit that concerns me is near the door, as in the picture will the mould lock in this little bit? 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search