By 111mattin111 - 12/4/2018 6:00:57 PM

Hi guys just about to take a mould of my roof the only bit that concerns me is near the door, as in the picture will the mould lock in this little bit? 
By 111mattin111 - 12/9/2018 7:57:12 PM

Steve Broad - 12/9/2018 3:48:29 PM
I am about to remake my roof, so have similar issues. At the moment my plan is to make a 3 piece mould, with the joins very close to the door recesses. Doing it this way keeps the main roof panel as a single piece, removing the risk of a join showing in the final part.

This is how I was thinking of maybe doing this mould the roof on one bit then both sides separate