Hi! 
So we have been using the post cure stated on the TDS sheet for EMP160/EG160. (1st image)
But I noticed on the video tutorial the post cure is completely different. (2nd image)

Our mould seems to be a lot darker than the mould that was shown on the video.

What cure cycles are you using for EMP160/EG160?

Please and thanks for the assistance! 