Stirred resin for 5 minutes then poured into another container and stirred for another 5 minutes.
Added a glasscast blue pigment and stirred for another couple of minutes to blend.
Done a 2mm pour and torched out bubbles but have observed this anomaly in a section of the pour.
Can someone tell me what’s going on here please?