5 minutes per bucket is typically about right. Technique is also important ie care taken to mix the whole ingredients not just "stirring" it but folding from top to bottom, scraping sides and base to ensure it is evenly mixed throughout.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|