Ok, now that I have pin hole free parts I now have another what seems insurmountable problem.

No matter what I have done I cannot get the clear to laydown without small craters in the outer surface of the clear. I am talking very, very small ones.

Here is what I have done.(and by the way I have been spraying clearcoat for years so I know how to do it, its just carbon panels that give me the problems)

1. Wash with soap and water - scuff with 600 or 400 wet and dry paper - wipe with prime wash -  spray. (pits)

2. Wipe with alcohol -scotch brite with grey ultra fine - wipe with 99.9% pure alcohol. (pits)

3. Scuffed as above - eliminated my spray equipment and sprayed clear with a spray bomb. (pits) 

4. Heated the part and spray bomb - sprayed fog coats - let flash well- built up to shiney. (pits)

5. Scuffed with "OLD DUTCH CLEANER" - sprayed with rattle can. (pits)

What the is going on!!!!! This is the pits!

Are you guys not getting these surface bleamishes ???????? 

The only thing that I can think of is that the carbon fiber is conductive of electricity or I am dealing with electrostatic repulsion.

I know that you cannot spray a plastic bumper without eliminating the electrostic fields.

Thanks for any help on this. Hopefully the Easy Composites Staff can clear this up!     Get It?  Clear this up!

Fred
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search