In terms of viscosity, you could get a thinner coat with the GlassCast 10, however it is not likely to lay as smoothly on the surface. GlassCast 3, because of its thickness and chemical additives, lays very smooth on a surface when poured thick enough. Going thinner means the surface will be less flat. With both resins you would still get i high gloss finish.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|