Group: Forum Members
Posts: 237,
Visits: 4.8K
|
You would make a tube with the ud running length ways so your length is immaterial you would cut material the same length as your mandrel How many times your ud would wrap around your tube depends it's diameter an how thick you want it Get to the end of your material just butt join another section on
|