Foam Core and Prepreg, thermal expansion


Author
Message
ISCmech-composite
ISCmech-composite
Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)
Group: Forum Members
Posts: 2, Visits: 368
I'm looking to make a part using Divinycell and prepreg, but I'm concerned with the thermal expansion of the foam causing poor bonding or internal stresses after cure. Does anyone have experience with using elevated temperature cure and a foam core such as Divinycell? I'm going to try to find a low temperature prepreg, but at best it would likely be 80C which is pushing the recommended processing temp on the data sheet which is 90C. 
Fasta
Fasta
Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
I cure pre preg on divinycell an other PVC  foams at 100C all the time, no film glues, no problems.




Steve Broad
Steve Broad
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
ISCmech-composite - 10/16/2018 2:20:37 AM
I'm looking to make a part using Divinycell and prepreg, but I'm concerned with the thermal expansion of the foam causing poor bonding or internal stresses after cure. Does anyone have experience with using elevated temperature cure and a foam core such as Divinycell? I'm going to try to find a low temperature prepreg, but at best it would likely be 80C which is pushing the recommended processing temp on the data sheet which is 90C. 

I have used this stuff many times with no adhesive film and with no issues. I tend to cure at around 120 deg C.

https://www.ecfibreglasssupplies.co.uk/product/airex-c70-75-structural-foam-10mm