Alan
A
Alan
posted 8 Years Ago
ANSWER
HOT
Topic Details
A
Group: Forum Members
Posts: 1,
Visits: 13
I am using glass cast 10 to cast pen blanks should I put it into my pressure pot after pouring if so @ what pressure and for how long
Look forward to reply
Alan
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Glass cast 10
agp244
-
8 Years Ago
Normally GlassCast does not need to be degassed or put in a pressure pot as the resin has a lot of self degassing properties so we would recommend letting it self degas first before considering using...
Warren (Staff)
-
8 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search