Normally GlassCast does not need to be degassed or put in a pressure pot as the resin has a lot of self degassing properties so we would recommend letting it self degas first before considering using a chamber or pressure pot.

However if you are still struggling with bubbles you certainly can degas or use a pressure pot. In our experience there is no limit or ideal level of pressure you should use and once under pressure, it should remain so until the resin has cured - the pressure pot works by crushing the bubbles into invisible size, so the pressure needs to be maintained.




Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Alan
A
Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)
Group: Forum Members
Posts: 1, Visits: 13
I am using glass cast 10 to cast pen blanks should I put it into my pressure pot after pouring if so @ what pressure and for how long
Look forward to reply
Alan
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search