Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Fabrication of templates
Fabrication of templates
Post Reply
Like
2
Fabrication of templates
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
svedberg
svedberg
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 22,
Visits: 173
Hi all!
I'm curious to know your best tips on the subject of making templates for the different pieces/panels of fabric used in a complicated (i.e. heavily double curved) mould?
I am in the process right now, using newspaper pages as the starting material, then proceeding with heavier florr protection paper as I' getting closerto the correct shape of each "panel" piece.
The actual GF/CF/Kevlar fabrics to be used when the real layup begins have of course very different draping properties than paper; is there a nice easy way to account for this in the making of templates? (the paper needs more cuts in it to properly accept the shape of the mould).
Would using cheap (similar weight) GF fabric for final try out of the shape of the templates in the mould be a good idea? I'd hate to find my CF/Kevlar cut into less than ideal shapes when layup time comes.
Thanks a lot!
/Lasse
Racing motorcycles!
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Fabrication of templates
svedberg
-
13 Years Ago
If you are planning to use 2/2 twill carbon say 200 g/sqm, then a glass fiber 2/2 twill with similar...
baja_patient
-
13 Years Ago
I may add to my post above that the layup planned is to be into a quite complicated mould. I'll be...
svedberg
-
13 Years Ago
Ahh... I see, I read this post after your other reply. If it is such a complex mould, and you wish...
baja_patient
-
13 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search