Hanaldo - 8/27/2018 11:19:31 PM
It's not really a process suited to infusion, which is why you wont find much about it. The general answer is it can only be done if you're using an internal flow media like Soric or 3D PET core, which obviously limits how thin your plates can be. Solid laminate wont work, you need a flow media.

Otherwise, pre-preg is dead easy.

many thanks for the response. Is there a good tutorial how to do it with pre-preg because I don't see any in the easycomposites youtube channel ?

Edited 7 Years Ago by S_Carbon_fibre
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
It's not really a process suited to infusion, which is why you wont find much about it. The general answer is it can only be done if you're using an internal flow media like Soric or 3D PET core, which obviously limits how thin your plates can be. Solid laminate wont work, you need a flow media.

Otherwise, pre-preg is dead easy.
S_Carbon_fibre
S
Supreme Being (154 reputation)Supreme Being (154 reputation)Supreme Being (154 reputation)Supreme Being (154 reputation)Supreme Being (154 reputation)Supreme Being (154 reputation)Supreme Being (154 reputation)Supreme Being (154 reputation)Supreme Being (154 reputation)
Group: Forum Members
Posts: 17, Visits: 89
Hello,

Is there a standard process to manufacture a two A-side carbon fibre plate? 
Ideally with Vacuum infusion. I still haven't found a tutorial or answer to this.

Many thanks for any hint.


GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search