Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
How deep are the pits? you can get pits from dust settling on the surface.
Also, if you coat the resin too thin, the surface will not be very smooth, it tends to pull and get dips and lumps when too thin.
Try and keep the room dust free as much as possible (or cover the part) and pour it so it is a minimum of around 1..5mm thick which is about 1.5kg per metre square.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|