By CampbellSA - 8/22/2018 7:24:47 AM

I did a third coat Glass Craft 3 on my first resin piece (800 x 400) last night and I checked it two hours later and was looking good - this morning it has several pits.

I did lots of preparation , I sanded it down to a flat smooth surface with a random orbital sander. I cleaned the surface many times , dried and blew it over with canned air. I washed it with acetone and made sure it was very dry. It was levelled out and pre heated before I did the pour. All the temps looked good and I made a cardboard box to cover it after the pour and I get this result. I am thinking that I have to change my brand of resin.

Simply can't carry on getting these results.
By CampbellSA - 8/27/2018 9:35:11 AM

Warren (Staff) - 8/23/2018 8:17:33 AM
Is the resin thinner on the end with the dips?? 

Might be localised contamination or the resin has just cast a bit too thin in that area.  Some pictures would help here.


Here's a picture of the pits ......

https://www.flickr.com/photos/156245622@N05/shares/J34W06