High Temperature Pre-Preg coat


Author
Message
Abilash
A
Forum Guru (59 reputation)Forum Guru (59 reputation)Forum Guru (59 reputation)Forum Guru (59 reputation)Forum Guru (59 reputation)Forum Guru (59 reputation)Forum Guru (59 reputation)Forum Guru (59 reputation)Forum Guru (59 reputation)
Group: Forum Members
Posts: 4, Visits: 38
Hi! So I'm designing a part that has to go over an exhaust of a car (not too near but not too far either) so it's got constant hot air blowing over it. I've been using pre-preg carbon fiber for the part and I was wondering if I could coat it with this:

https://www.youtube.com/watch?v=-R7mm63eWv8

which I came across while browsing the internet. Was wondering what you guys would think of this if I used it as my surface gel coat for my pre-preg parts.

Thank you!
Edited 8 Years Ago by Abilash
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Quite a few pre-preg systems have a working temperature after postcure in the 120 -130 C ball park so I can't see the advantage of using this coating.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Steve Broad
Steve Broad
Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Agreed, seems to be a pretty pointless product for epoxy impregnated carbon cloth, probably mainly used for vinylester resins and fibreglass :-)

I have prepreg carbon using epoxy resin capable of coping with 220 deg C. The lowest I am aware of is 125 deg C
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
X-Preg service temp is only 115C ^


The product in the video is basically an epoxy tooling gelcoat, it's intended for high temperature tooling - ie. moulds for pre-preg.

There is no point putting a high temperature surface coat on a laminate that cant handle those same temperatures. If your pre-preg parts cant handle more than 120C then having a surface coat that can handle 200C isn't going to do anything for it.
Steve Broad
Steve Broad
Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Hanaldo - 8/13/2018 11:18:19 PM
X-Preg service temp is only 115C ^


The product in the video is basically an epoxy tooling gelcoat, it's intended for high temperature tooling - ie. moulds for pre-preg.

There is no point putting a high temperature surface coat on a laminate that cant handle those same temperatures. If your pre-preg parts cant handle more than 120C then having a surface coat that can handle 200C isn't going to do anything for it.

As the surface coat isn't a heat reflector, good point.

An option is to apply a heat reflective material, such as something from the Zircotec range. They do a self adhesive option.

https://www.zircotec.com/zircoflex/zircoflex-i/