Hi, 
I've having issues with bridging when trying to do a 5mm thick carbon/kevlar shell for a robot project of mine, im a machinist and have done fibreglass moulds for customers before but never a carbon fibre one, i think i rushed into machining the mould has i thought i would be able to wet lay carbon fibre sheet and resin like fiberglass, i've had 2 failed attempts trying to wet lay with struggling to get the fabric into all the contours with trying to get a quite thick wall thickness, i phoned easy and they said resin infusion is the way to go with using a tack spray to hold the fabric is place until the vacuum and resin is in, i purchased the kit and have tried the infusion but i think i haven't left enough flange around the base to have excess fabric pull its way down has i've had a better finish but still bridging/not taking the full shape, could this be the issue?, i can machine another mould with a 50mm flange around rather than the 25mm i have at the moment 



Thanks
Andy
Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Dont get me wrong, I'm all for pre-preg! I use it for most applications. I just dont think it's necessary for this job, and isn't really any more suitable than infusion is. Hes already bought the infusion kit, so for me there's no point investing more money in a different setup.
Steve Broad
Steve Broad
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Hanaldo - 8/6/2018 12:48:33 AM
Dont get me wrong, I'm all for pre-preg! I use it for most applications. I just dont think it's necessary for this job, and isn't really any more suitable than infusion is. Hes already bought the infusion kit, so for me there's no point investing more money in a different setup.

I don't :-) and as he has the stuff he may as well use it. I had planned to use infusion for my car's roof and front clip and bought all the hardware and consumables (still have them :-( ), but then discovered prepreg was so much easier and less messy. Just had to build an oven big enough Smile

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
K3 - 7 Years Ago
drippy - 7 Years Ago
Steve Broad - 7 Years Ago
Hanaldo - 7 Years Ago
Steve Broad - 7 Years Ago
Hanaldo - 7 Years Ago
Steve Broad - 7 Years Ago
K3 - 7 Years Ago
Steve Broad - 7 Years Ago
Furrari - 7 Years Ago
Furrari - 7 Years Ago
drippy - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search