Hi, 
I've having issues with bridging when trying to do a 5mm thick carbon/kevlar shell for a robot project of mine, im a machinist and have done fibreglass moulds for customers before but never a carbon fibre one, i think i rushed into machining the mould has i thought i would be able to wet lay carbon fibre sheet and resin like fiberglass, i've had 2 failed attempts trying to wet lay with struggling to get the fabric into all the contours with trying to get a quite thick wall thickness, i phoned easy and they said resin infusion is the way to go with using a tack spray to hold the fabric is place until the vacuum and resin is in, i purchased the kit and have tried the infusion but i think i haven't left enough flange around the base to have excess fabric pull its way down has i've had a better finish but still bridging/not taking the full shape, could this be the issue?, i can machine another mould with a 50mm flange around rather than the 25mm i have at the moment 



Thanks
Andy
Reply
Steve Broad
Steve Broad
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
OOA Aramid/Carbon mix :-)



Rarely use the wet stuff these days, so messy and time constrained unless using infusion (which is a bit of a faff IMO) There are even prepregs that don't need to be kept in a freezer!

However, each to his own :-)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
K3 - 7 Years Ago
drippy - 7 Years Ago
Steve Broad - 7 Years Ago
Hanaldo - 7 Years Ago
Steve Broad - 7 Years Ago
Hanaldo - 7 Years Ago
Steve Broad - 7 Years Ago
K3 - 7 Years Ago
Steve Broad - 7 Years Ago
Furrari - 7 Years Ago
Furrari - 7 Years Ago
drippy - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search