Does epoxy hardner go bad?


Author
Message
darknight7777777
darknight7777777
Supreme Being (195 reputation)Supreme Being (195 reputation)Supreme Being (195 reputation)Supreme Being (195 reputation)Supreme Being (195 reputation)Supreme Being (195 reputation)Supreme Being (195 reputation)Supreme Being (195 reputation)Supreme Being (195 reputation)
Group: Forum Members
Posts: 7, Visits: 254
As thread title.

I have some fast hardner in the container it comes in from EC and it has gone dark. I only realised when I had a new set delivered with my infusion resin.

My workshop has a constant 22-23 degrees temp and only on a rack away from sunlight. 

Also is ok to mix equal amounts of fast and slow hardner to give me a little more time before my resin gels and not completes full infusion.

Thanks