How do I Vaccum Bag this Air Box ??


Author
Message
oekmont
oekmont
Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
If it's really 15 °C, it is about 10° too could at your place.

Hanaldo
Hanaldo
Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Cut the bristles on your brush down to about an inch long, this will make it much easier to work. Make sure to pull out any loose bristles before applying the gelcoat.
Eddie Walsh
E
Supreme Being (616 reputation)Supreme Being (616 reputation)Supreme Being (616 reputation)Supreme Being (616 reputation)Supreme Being (616 reputation)Supreme Being (616 reputation)Supreme Being (616 reputation)Supreme Being (616 reputation)Supreme Being (616 reputation)
Group: Forum Members
Posts: 52, Visits: 294
oekmont - 1/18/2019 11:49:33 AM
If it's really 15 °C, it is about 10° too could at your place.

Hi Thanks, sounds like I will have to take it to Bed with me ??, at least it goes off in my workshop which is just about 10 degrees C, so is there no way of thinning it out so it would spread a lot easier, again thanks, regards DM

oekmont
oekmont
Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
No, not really. You should definitely not work at these temperatures. Especially not with high temp resins.
First: they tent to be thicker, wich makes them paste like at low temperatures. This means it is much more likely to trap air inside corners and inside the resin itself.
Secondly: if you use high temp resin you will likely heat the mould up to higher temperatures. This will let the trapped air expand, and ruin your mould surface.
It was you, who wanted to vacuum the mould, because he was fearing he would need to repair it because of trapped air, right? Working at low temperatures  is the most reliable way to cause exactly that.

Eddie Walsh
E
Supreme Being (616 reputation)Supreme Being (616 reputation)Supreme Being (616 reputation)Supreme Being (616 reputation)Supreme Being (616 reputation)Supreme Being (616 reputation)Supreme Being (616 reputation)Supreme Being (616 reputation)Supreme Being (616 reputation)
Group: Forum Members
Posts: 52, Visits: 294
oekmont - 1/18/2019 12:57:49 PM
No, not really. You should definitely not work at these temperatures. Especially not with high temp resins.
First: they tent to be thicker, wich makes them paste like at low temperatures. This means it is much more likely to trap air inside corners and inside the resin itself.
Secondly: if you use high temp resin you will likely heat the mould up to higher temperatures. This will let the trapped air expand, and ruin your mould surface.
It was you, who wanted to vacuum the mould, because he was fearing he would need to repair it because of trapped air, right? Working at low temperatures  is the most reliable way to cause exactly that.

Hi, Thanks again for the advice, but I have started so now I will have to finish as best I can, that was why I asked if there was any way of thinning it down, so is there any way to thin it down, Regards DM

oekmont
oekmont
Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
=> no, not really. Except for temperature elevation.

Hanaldo
Hanaldo
Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yeh these sorts of epoxies are 100% solids - there are no solvents in them, and you cant add solvents to them. Only way to lower the viscosity is with heat.
Eddie Walsh
E
Supreme Being (616 reputation)Supreme Being (616 reputation)Supreme Being (616 reputation)Supreme Being (616 reputation)Supreme Being (616 reputation)Supreme Being (616 reputation)Supreme Being (616 reputation)Supreme Being (616 reputation)Supreme Being (616 reputation)
Group: Forum Members
Posts: 52, Visits: 294
Hanaldo - 1/18/2019 5:25:05 PM
Yeh these sorts of epoxies are 100% solids - there are no solvents in them, and you cant add solvents to them. Only way to lower the viscosity is with heat.

Hi All again, Thanks for the advice, I will let you know how it turns out whether it is good or bad news, Regards DM

Eddie Walsh
E
Supreme Being (616 reputation)Supreme Being (616 reputation)Supreme Being (616 reputation)Supreme Being (616 reputation)Supreme Being (616 reputation)Supreme Being (616 reputation)Supreme Being (616 reputation)Supreme Being (616 reputation)Supreme Being (616 reputation)
Group: Forum Members
Posts: 52, Visits: 294
Eddie Walsh - 1/18/2019 10:37:18 PM
Hanaldo - 1/18/2019 5:25:05 PM
Yeh these sorts of epoxies are 100% solids - there are no solvents in them, and you cant add solvents to them. Only way to lower the viscosity is with heat.

Hi All again, Thanks for the advice, I will let you know how it turns out whether it is good or bad news, Regards DM

Hi All, I have just spent most of the day trying to roll out the first layers of Mat on my mould ???, what it seemed like is the Epoxy Resin wasn't dissolving the Powder Binder in the Mat so I was just chasing large air pockets under my mat ?? eventually got it so it does not look too bad but definitely not perfect, I never had anything like this with Polyester, I suppose I was lucky temp was still low or it would have cured before I got it to a resonable state, again any help or advice appreciated, Regards DM

oekmont
oekmont
Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
Epoxy doesn't dissolve usual binders, because it doesn't contain solvents. In tooling applications epoxy is usually used in combination with woven cloth. The first layer of a mould would be something like 160 g/m^2 glass cloth.
Or is it a special epoxy compatible mat? They behave different than standard csm in polyester. In direct comparison the word "worse" would describe it best. But not as bad as you described.

To be honest, I would recommend to let it cure and start again with proper planning and testing.

Edited 7 Years Ago by oekmont
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search