Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Bonding oddly shaped HDPE tank with HDPE sheets
Bonding oddly shaped HDPE tank with HDPE sheets
Post Reply
Like
4
Bonding oddly shaped HDPE tank with HDPE sheets
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
fullmetal7777
f
fullmetal7777
posted 8 Years Ago
ANSWER
HOT
Topic Details
f
Group: Forum Members
Posts: 2,
Visits: 7
I'm using this
Rhino Containment Vessel
as a sump for my large aquarium and I need to be able to bond hdpe sheets to the sides of the tank to make shelves. The tank itself has a textured side, so I know I might need to do some sort of fiberglassing? Only an example, not sure if fiberglassing would be the way to go in this situation, but do you guys have any ideas?
Thanks
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Bonding oddly shaped HDPE tank with HDPE sheets
fullmetal7777
-
8 Years Ago
HDPE is an inert low energy plastic and as such you generally need specialist adhesives to bond to it. I doubt you would get a decent grip using polyester or epoxy based resins and fibreglass.
Warren (Staff)
-
8 Years Ago
Bummer, back to the drawing board I guess, Thanks!
fullmetal7777
-
8 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search