Warren (Staff) - 6/29/2018 8:33:29 AM
HDPE is an inert low energy plastic and as such you generally need specialist adhesives to bond to it.  I doubt you would get a decent grip using polyester or epoxy based resins and fibreglass.

Bummer, back to the drawing board I guess, Thanks!

Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
HDPE is an inert low energy plastic and as such you generally need specialist adhesives to bond to it.  I doubt you would get a decent grip using polyester or epoxy based resins and fibreglass.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
fullmetal7777
f
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 2, Visits: 7
I'm using this Rhino Containment Vessel as a sump for my large aquarium and I need to be able to bond hdpe sheets to the sides of the tank to make shelves. The tank itself has a textured side, so I know I might need to do some sort of fiberglassing? Only an example, not sure if fiberglassing would be the way to go in this situation, but do you guys have any ideas?

Thanks