Group: Forum Members
Posts: 1,
Visits: 9
|
Hello!
I have two questions:
I have a vacuum pump and ordered some vacuum bags from easycomposites. But I am not sure how to avoid that the vacuum bag doesn't glue to the surface of the carbon fibre? As I think it is narly impossible that not a drop at all of the resin goes through the carbon fibre. Some advice would be very apreciated.
Another question is how to prepare the part to be clear coated? Stopping with sanding with a 1000 sand papier and then adding the clear cat straight?