hi guys,

i tried to skin a plastic piece about 1sq meter. i used carbon base coat, then diolen and after that layer of  carbon fibre laminating epoxy resin. i applied laminating epoxy with plastic card. so far so good. after 48 hours i tried to apply second layer (same technique) but after 5 minutes of flattening with card the epoxy started to be white/milky (i guess because of micro air bubles). 
the result is that diolen is not visible because second layer is milky. 
the rest of epoxy i didn't use is on picture (surplus epoxy from board i put back to mixing pot). 
next day the surplus epoxy in mixing pot hasn't flat surface and had bilions microair bubles.

i am sure i did something wrong but don't know what... at the begining the epoxy had some air bubles (only few as usual) but when i started a work with plastic card it became to have more and more air bubles and result was the whole epoxy was white.
do you have any similar experience pls? 

your help is more than appreciated
ondrej


Attachments
photo.JPG (465 views, 413.00 KB)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search