			            I would like to know exactly what the plastic card was, i once used a piece of plastic cut from an ice cream tub to smooth out epoxy, i smoothed really well but something made micro bubbles appear on that job (not as badly as in your pot !!) and the only thing i thought i had done differently was to use the soft plastic spreader. ? !. I dont use it anymore, i think you have to very careful when adding anything particuly other untried plastics to a resin curing environment.                
			            				
			                                 
                     
                                            
                         
                    
                  
             |