Dear Matt
My name is Weera .I am in Thailand.
Your video inspired me work the carbon hood.
I want to make he mold for resin infusion technique.
I can not find the good source compare to to yours.
Question
1.If I brush gelcoat , the infused resin to make the mold?
Bcoz sale person recommend me to spay gelcoat to avoid the league.

2.If I brush the gelcoat , then hand lay=up as you do.
How many hood that I can make from the mold?
What is your advised Matt...
Thank you for Matt and anyone who advised me.
Extreme
Extreme
Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)
Group: Forum Members
Posts: 17, Visits: 78
Matt,

Can you please tell me why in your video you use GC50 Epoxy Compatible Ployester Gelcoat and not just your regular Clear Epoxy Gelcoat ?

thank you,

Erick
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Another idea if your parts are too big for an oven is a modern temperature regulated heat blanket. I used one when I first made a bonnet at home and it achieved a mould surface temperature of 40 Celcius when placed on the complete infused mould layup, then wrapped in a duvet to reduce heat loss.

Although modern electric blankets have a thermal cut out and are designed to be left unsupervised, I would always recommend keeping a close eye on it as it isnt being used as the manufacturer intended.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Andy,

A post-cure in the mould would be a very good thing to do to ensure that there is no danger of the part distorting. 60'C for 6hrs would be a good post cure, after that there should be no danger of the part distorting in the sun.

If you need to post cure out of the mould then the recommendation would be to increase the temperature very gradually over  along period of time. This will reduce the amount of out of mould distortion.

All the best, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
andygtt
andygtt
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Forum Members
Posts: 157, Visits: 1.2K
Id very much like black soric... with the curved shapes I make the soric is always visable to my critical eye.

I have a technical query on resin infusion... if you were to paint this part, would it need to be oven cured in the mould.

If you decided to fit this part without oven baking, then later paint it, is there a possibility it will soften and loose its shape... ie would you need to reintroduce t to the mould and put it in an oven first and then paint it?

I dont want the part to loose shape in extreme sunlight and I really want it painted and oven cured.
Warren
Warren
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Administrators
Posts: 214, Visits: 783
GC50 can be applied by brush but its not ideal with resin infusion as the weave will look slightly out of place on the uneven surface.  So it is recommended to be sprayed.

However for wet lay, the carbon will "float" on a layer of resin so the unevenness associated with brush application of the gel coat is hardly noticable if at all.
Extreme
Extreme
Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)
Group: Forum Members
Posts: 17, Visits: 78
Warren,

Can the UV protective gelcoat be brushed in? I imagine it's propabably best to spray it, but just wondering.

I have to say I really like your companies helpful videos.

Thank you,

Erick
Warren
Warren
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Administrators
Posts: 214, Visits: 783
The gelcoat is done to provide a improved surface finish and also to give UV protection without the need to lacquer the part.

By using a core you can use less layers of fabric (and hence save money) yet still have a stiff and light panel.
Extreme
Extreme
Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)
Group: Forum Members
Posts: 17, Visits: 78


This is my first post so I would like to start out by saying thank you easycomposites for all the information you provide.

Matt, Ihave watched the videos in regards to resin infusion and I have a couplequestions.

Whyon the carbon fiber hood/bonnet did you spray clear gel coat before the firstlayer? I noticed this was not done on the other resin infusion video.

Alsowhy was a infusion core material used on the hood/bonnet? Is this necessary onlarge parts? Is it for strength to the part or strictly to help the resin flow?Could covering the entire part with Infusion mesh have the same effect?

Ican't wait to start making parts for my car.

Thankyou,

Erick


brasco
brasco
Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)
Group: Forum Members
Posts: 192, Visits: 305
i am a bmw 325 nut...of the 80's models and their hood is about 45 pounds and in CF it should be 5 pounds? --yes the weight difference is that big !!
it is a greater difference than 2 hoods (like a ford ranger) where both an aluminium and steel version are available. the aluminium is crazy light, and the CF is x10 beyond that !!


CarbonFiberCreations



GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search