Carbone tube - angle


Author
Message
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
You could potentially buy straight tubes and do a mitre joint on them, then bond them together with epoxy and some loose carbon strands. 

But it sort of depends what you're using them for and how strong they need to be, tolerances etc. Those are pretty small tubes, so it would also be quite fiddly without a jig to hold the tubes while you bonded them.
Steve Broad
Steve Broad
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Damien Coudreuse - 5/8/2018 9:52:03 AM
Hi all,

I  would like to fabricate small connnectors in carbone...I need tubes of 6 and 8 mm diameter that make a 90 angle...is that easy/possible ? Or is there a way to get straight carbone tubes and bend them ?

Thanks !

Look at RC and Drone supply sites. They do various tube connectors, but they aren't cheep and mostly not made from carbon. Carbon connectors seem to be around £40 each!

You can't bend carbon tubes :-)

Damien
Damien
Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)
Group: Forum Members
Posts: 32, Visits: 132
Hi all,

I  would like to fabricate small connnectors in carbone...I need tubes of 6 and 8 mm diameter that make a 90 angle...is that easy/possible ? Or is there a way to get straight carbone tubes and bend them ?

Thanks !

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search