The resin has got cold at some point and crystalised. Don't worry, it is not damaged and is completely reversible.
Sticking it on a hot radiator, oven at 50C or in a sink of hot water for a few hours (lids sealed) is usually enough heat energy to turn it back to a liquid.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|