By markbaggy - 5/4/2018 9:47:29 AM
Hi guys,
ive just opened a new bottle of glasscast 50 resin to find its cloudy and almost a bit crystallized in places. is this normal and if not why is it like this? its been stored inside at around 20 degrees unopened for a couple of weeks.
any help will be appreciated
|
By Warren (Staff) - 5/4/2018 1:11:40 PM
The resin has got cold at some point and crystalised. Don't worry, it is not damaged and is completely reversible.
Sticking it on a hot radiator, oven at 50C or in a sink of hot water for a few hours (lids sealed) is usually enough heat energy to turn it back to a liquid.
|
|