Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The balance issues are why they are often not repaired as Okemont says.  However technically it can be physically repaired in a similar way to a tube repair, although with having to remove and restring it is a lot of effort for these days what is usually a cheap imported product.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
oekmont
oekmont
Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
A co-worker of mine once repaired a badminton racket for our sales manager, wich played badminton at a fairly high level. While it worked fine as a structual repair, our sales manager didn't use it any more, because the balance and dynamic behaviour was now far off. So badminton rackets are one of these products I consider unrepairable.

bat and bal
bat and bal
Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)
Group: Forum Members
Posts: 1, Visits: 1
Dear SIr 


This is Sakir, I would like to know more about your products, Can we repair Badminton Racquets with this products ? do you have any demo videos on Youtube?


Best Regards  
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search