Hi Warren/guys

I've recently bought some of the new Clearpol polyester gelcoat to do a little bit of fibreglass work and noticed that it is very thin compared to other gelcoats I've used and smells somewhat different too which, I guess, is down to the particular formulation

It was well mixed prior to adding catalyst but fish-eyed very readily and didn't adhere too well to vertical sides, leading me to have to keep brushing over and apply a second coat. Its consistency was more like a resin than a gelcoat. Is it formulated for spraying ideally or is the low viscosity I've seen unusual?

Thanks
Edited 8 Years Ago by MarkMK