You state that The GC50 Epoxy Compatible Gelcoat is ready for the application of the epoxy laminate, resin infusion, within 2-3hrs (@25°C) but also remains bondable for up to 24hrs making it easy to achieve optimum bond strength.
Is it possible to make the gelcoat bondable after 48hrs.?
-    If so then how?
If the temperature only is (@15°C), how long time is the gelcoat bondable?