Steve Broad
Steve Broad
posted 8 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 408,
Visits: 4.1K
What are the pros and cons of using 2 layers of 210gsm against 1 layer of 416gsm, apart from price and ease of forming :-) ?
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
One v Two layers
Steve Broad
-
8 Years Ago
Theoretically speaking, two layers of the 210g would result in a laminate with less crimp, making it stronger. Realistically, this is such a marginal difference that it is really irrelevant for almos...
Hanaldo
-
8 Years Ago
Thanks for reply Here is the mould I will be using :-) Additional layers and reinforcing ribs will be added where extra strength is required. I discussed the advantage of alternating the weave...
Steve Broad
-
8 Years Ago
For simple body panels, go with the single layer of 416gsm rather than 2 layers of 210gsm. The mechanical difference will not be significant in the application you are using it for but the cost...
Warren (Staff)
-
8 Years Ago
Thanks Warren.
Steve Broad
-
8 Years Ago
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search