Hi everyone! Just  a quick one,

I am trying to make a carbon fibre snare drum with the infusion technic but don´t know which resin would be appropriate.

I know epoxi gives the best mechanical characteristics but... will I really need that strength for a snare drum?

Polyester is significantly cheaper and, for me, the handling easier. Would it be a better choice?

Thank you in advance to everyone.

Cheers

 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
MarcosTG - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search