Hi
Can I use clear cast resin to make a two part mould
It will be task 12 that i shall be pouring into the mould
Kind regards
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Although you could use one of the GlassCast resins to make a mould, for pouring in a PU resin, you would probably be better off with an Addition Cure Silicone such as our AS40 silicone.  With Silicone you would not need a release agent and the flex of the silicone would help de-moulding.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search