By Roxylass - 3/16/2018 9:37:30 PM
Hi Can I use clear cast resin to make a two part mould It will be task 12 that i shall be pouring into the mould Kind regards
|
By Warren (Staff) - 3/19/2018 10:55:00 AM
Although you could use one of the GlassCast resins to make a mould, for pouring in a PU resin, you would probably be better off with an Addition Cure Silicone such as our AS40 silicone. With Silicone you would not need a release agent and the flex of the silicone would help de-moulding.
|
|