scottracing - 3/12/2018 10:13:48 PM
How well will this pass the very stringent FST requirements for rail? I have worked on rail applications and its either phenolics or thermoplastics, this is a very good idea though as the floors in trains are still made from wood.


Hi Scott Racing, would love to hear more about your experience in your rail, and how you see composites being integrated into subways/long-distance trains in the next few years?

scottracing
scottracing
Supreme Being (5.9K reputation)Supreme Being (5.9K reputation)Supreme Being (5.9K reputation)Supreme Being (5.9K reputation)Supreme Being (5.9K reputation)Supreme Being (5.9K reputation)Supreme Being (5.9K reputation)Supreme Being (5.9K reputation)Supreme Being (5.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
How well will this pass the very stringent FST requirements for rail? I have worked on rail applications and its either phenolics or thermoplastics, this is a very good idea though as the floors in trains are still made from wood.


JEC Composites
J
Supreme Being (178 reputation)Supreme Being (178 reputation)Supreme Being (178 reputation)Supreme Being (178 reputation)Supreme Being (178 reputation)Supreme Being (178 reputation)Supreme Being (178 reputation)Supreme Being (178 reputation)Supreme Being (178 reputation)
Group: Forum Members
Posts: 15, Visits: 42
Matthieu Libeert - 3/12/2018 7:52:15 PM
JEC Composites - 3/12/2018 5:21:35 PM
Hello all,


We thought we would share this interesting article about a carbon fiber subway car which is 35% lighter than the traditional metal ones:

http://www.jeccomposites.com/knowledge/international-composites-news/china-develops-subway-car-made-carbon-fiber

There are lots of great benefits to this new car. How long do you all think it is before we see these on the tracks?

Thanks for sharing! hope the price of carbon fiber wont rise with all the carbonfiber they will need BigGrin

Hi Matthieu, do you work with composites in transportation, or in another area? 

Matthieu Libeert
Matthieu Libeert
Supreme Being (10K reputation)Supreme Being (10K reputation)Supreme Being (10K reputation)Supreme Being (10K reputation)Supreme Being (10K reputation)Supreme Being (10K reputation)Supreme Being (10K reputation)Supreme Being (10K reputation)Supreme Being (10K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
JEC Composites - 3/12/2018 5:21:35 PM
Hello all,


We thought we would share this interesting article about a carbon fiber subway car which is 35% lighter than the traditional metal ones:

http://www.jeccomposites.com/knowledge/international-composites-news/china-develops-subway-car-made-carbon-fiber

There are lots of great benefits to this new car. How long do you all think it is before we see these on the tracks?

Thanks for sharing! hope the price of carbon fiber wont rise with all the carbonfiber they will need BigGrin


Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




JEC Composites
J
Supreme Being (178 reputation)Supreme Being (178 reputation)Supreme Being (178 reputation)Supreme Being (178 reputation)Supreme Being (178 reputation)Supreme Being (178 reputation)Supreme Being (178 reputation)Supreme Being (178 reputation)Supreme Being (178 reputation)
Group: Forum Members
Posts: 15, Visits: 42
Hello all,


We thought we would share this interesting article about a carbon fiber subway car which is 35% lighter than the traditional metal ones:

http://www.jeccomposites.com/knowledge/international-composites-news/china-develops-subway-car-made-carbon-fiber

There are lots of great benefits to this new car. How long do you all think it is before we see these on the tracks?