bmastino
b
bmastino
posted 8 Years Ago
ANSWER
HOT
Topic Details
b
Group: Forum Members
Posts: 3,
Visits: 4
I am creating a bottle top shower floor. What would be the best GlassCast product to use?
Thanks
Bridget
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Bottle Top Shower Floor
bmastino
-
8 Years Ago
Is this for the shower room floor or the actual shower tray itself? Typically the GlassCast 3 Clear Epoxy Coating Resin is the resin to go for when coating floor surfaces such as bottle tops and...
Warren (Staff)
-
8 Years Ago
It is for a wet room in a campervan so will only be used occassionally... Could I use GlassCast and then apply a tile sealant over the top to be sure? Thanks
bmastino
-
8 Years Ago
As long as your sealant will adhere to the epoxy, then i see no reason why that wouldn't work as it would in effect protect the resin from the water.
Warren (Staff)
-
8 Years Ago
Great! Thanks!
bmastino
-
8 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search