+x Warren (Staff) - 3/13/2018 10:05:40 AM+x bmastino - 3/12/2018 4:40:36 PMIt is for a wet room in a campervan so will only be used occassionally...Could I use GlassCast and then apply a tile sealant over the top to be sure?ThanksAs long as your sealant will adhere to the epoxy, then i see no reason why that wouldn't work as it would in effect protect the resin from the water.
+x bmastino - 3/12/2018 4:40:36 PMIt is for a wet room in a campervan so will only be used occassionally...Could I use GlassCast and then apply a tile sealant over the top to be sure?Thanks