I am about to finish a small table top with glass cast 3, having never used it before. The datasheet advises 1kg of resin/sqm/mm and a ratio of 2:1. However I note that the kits come as what look like ratios, e.g. 0.5kg = 333g resin and 167g hardner (i.e. 2:1 ratio), etc. Can I just clarify please before I mix, for a 1mm thickness over 1sqm do I need 1kg of final mix or 1kg of resin + 500g hardner.
Sorry if this is a silly question but better to clarify now than find out afterwards! Thank you.
|