small indentation keep appearing overnight
small indentation keep appearing overnight
Post Reply
Like
5
small indentation keep appearing overnight
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Glen Sturman
Glen Sturman
posted 8 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 1
Using glass cast on a table, resin appears to be very clear. Leaving it overnight and very small indentations keep appearing.
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
small indentation keep appearing overnight
Glen Sturman
-
8 Years Ago
what sort of surface are you casting over? if is wood and if so has it been sealed? Are the indents random or in the same places?
Warren (Staff)
-
8 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search