By Glen Sturman - 2/25/2018 6:19:50 PM
Using glass cast on a table, resin appears to be very clear. Leaving it overnight and very small indentations keep appearing.
|
By Warren (Staff) - 2/26/2018 10:02:36 AM
what sort of surface are you casting over? if is wood and if so has it been sealed? Are the indents random or in the same places?
|
|